SHS Al Alloy 7042™
SHS Al Alloy 7042™
Technology Highlights
- The alloy 7042 in T6 temper (7042-T6) has excellent strength and toughness in the temperature range from -450°F to 250°F.
- Direct chill cast 7042-T6 has mechanical properties which are similar to the properties of 7075-T6 or 7050-T74 forgings, at superior stress-corrosion resistance.
- Extruded 7042-T6 products have ~30% higher specific strength than Ti alloys.
- Forged products made of 7042-T6 are 25-35% stronger and tougher than similar forgings made of 7075-T6 and 7050-T74.
7042
- Currently available in two conditions:
- Direct chill cast billets (F temper)
- Extruded bars (T6 temper)
- Requests for forged or rolled products can also be negotiated on individual basis.